Injection molding defects manufacturing guide

Common Injection Molding Defects and Solutions

Injection molding defects typically arise from four factors: material, process, mold, and machine. This guide covers 28 common defects, prioritized for quick on-site troubleshooting.

Change this Subheading

Image Box Title

Change this description

QQ20260605 174839

Part 1: Surface/Appearance Defects

DefectDescriptionKey Solutions
1. Sink MarksLocal surface depressionIncrease pack/hold pressure & time; enlarge gate; optimize rib thickness (≤0.6× wall)
2. Charred StreaksSilver/brown streaksReduce injection speed; avoid sharp corners; check material drying
3. Moisture StreaksWavy silver streaksPre-dry material thoroughly; increase mold temp; lower melt temp
4. Air StreaksGrooves, dots or lines on surfaceAdd/deepen vents; adjust injection speed; change gate location
5. Colored StreaksInconsistent colorIncrease back pressure; lower melt temp; use mixing screw
6. Glass Fiber StreaksRough surface, exposed fibersRaise mold/melt temp; inject faster; use shorter glass fibers
7. Gloss DifferencesMatte or shiny spotsIncrease and balance mold temp; raise pack pressure; optimize transfer point
8. JettingSnake-like pattern near gateReduce injection speed; enlarge gate; raise melt/mold temp
9. Record GroovesWavy ripples on surfaceIncrease injection speed/pressure; raise melt/mold temp
10. Dull Spots Near GateShadow near gateReduce speed near gate; enlarge gate; add radius transition

Part 2: Internal/Filling Defects

DefectDescriptionKey Solutions
11. BlisteringRound/oval internal voidsVacuum: lower speed, increase pack pressure; Gas: dry material, increase back pressure
12. VoidsIrregular cavities in thick sectionsLocate gate at thickest wall; avoid sudden wall thickness changes
13. Short ShotIncomplete fillingIncrease injection pressure/speed/temp; enlarge gate; improve venting
14. Weld LineVisible line where flows meetRaise melt/mold temp/speed; add venting; use overflow tab
15. Cold SlugsHardened material lumpsCheck nozzle temp; add cold well; adjust decompression
16. Dark SpotsBlack spots on light partsClean screw/barrel; check material for contaminants; lower melt temp

Part 3: Deformation/Mechanical Defects

DefectDescriptionKey Solutions
17. WarpageOverall part distortionBalance cooling; optimize gate location; adjust packing; balance ejection
18. Deformation During DemouldingBending/collapse on ejectionIncrease cooling time; lower pack pressure; add ejector area; check undercuts
19. Visible Ejector MarksWhite marks at ejector pinsIncrease ejector count/area; add draft angle; lower pack pressure
20. Ejection GroovesScratch lines on side wallsIncrease cooling time; increase draft angle; polish in ejection direction
21. Stress Whitening/CracksWhite marks or cracksLower pack pressure; optimize ejection; add radii to part design
22. Broken Film HingeHinge fractureMove gate away from hinge; raise mold temp; increase hinge thickness moderately
23. Flaking of Surface LayerLayer separationCheck material purity/compability; optimize plastication; reduce injection speed

Part 4: Other/Process Defects

DefectDescriptionKey Solutions
24. Diesel Effect (Burner)Local burning (yellow/black)Reduce injection speed; add venting; change flow pattern
25. FlashExcess plastic at parting lineIncrease clamp force; reduce injection/pack pressure; repair mold
26. FilamentationStringy plastic near gateLower nozzle temp; increase cooling time; check hot runner
27. Plate OutDeposits on mold/vent surfacesLower melt temp; shorten cycle time; check additive compatibility
28. Electroplated Part DefectsBlisters/cracks after platingReduce molded-in stress; dry material thoroughly; avoid sharp corners; use high-gloss mold finish

Quick Troubleshooting Checklist

  1. المادة – Is it properly dried? Free of contaminants?
  2. Mold – Are vents sufficient? Is gate design appropriate?
  3. العملية – Adjust in this order: temperature → speed → pressure. Change only one parameter at a time.
  4. Machine – Is screw non-return valve worn? Is barrel temperature stable?

هل تحتاج إلى أجزاء مصبوبة بالحقن عالية الجودة؟

إذا كان لديك فكرة رائعة، يمكننا مساعدتك على تحقيقها. لقد قمنا بذلك من قبل ونستمتع بأن نصبح شركاء طوال عملية إنشاء المنتج. من تقديم النصيحة لك خلال عملية الحصول على القالب إلى تسليم منتجك الجديد للعملاء، نريد العمل معك في كل خطوة على الطريق.

السعي الدائم للتحسين

قوتنا هي مرونتنا وقدرتنا على التكيف. نحن نجمع بين تجربتنا وأفكارك لطرح منتجات تتقدم خطوة نحو المستقبل.

جودة الإنتاج الخالية من العيوب

رؤيتنا ليست فقط تقديم منتجات تفوق توقعات العملاء ولكن أيضًا مساعدتهم على خفض التكاليف من خلال العمل معهم في مجال تصميم القوالب. 

تسليم الطلبات في الوقت المحدد 

نرغب في ضمان استلام العملاء للبضائع بدقة وإكمال التسليم في أقصر وقت ممكن.